Advantage:
1. Less blowhole inside the casting, which can be heat treated.
2. The mold has long life and low cost.
3. High elongation rate.
4. The process is relatively simple.
Disadvantage:
1. Slow filling and low production efficiency.
2. Relying on liquid self-weight molding, the product has low density and slightly weak strength.
3. The surface smoothness of the product is not high.
4. Not suitable for producing thin-walled parts.
Applicable:
Apply to products with large wall thickness, such as steering knuckles, control walls and other chassis safety parts.